Chemical Specifications




NEW ZEALAND GAZETTE, No. 50 — 8 MAY 2015

(f) mercury (mg/kg)—maximum 0.1;
(g) hexane (mg/kg)—maximum 0.3.

S3–21 Specification for oil derived from marine micro-algae (Schizochytrium sp.) rich in docosahexaenoic acid (DHA)

For oil derived from marine micro-algae (Schizochytrium sp.) rich in docosahexaenoic acid (DHA), the specifications are the following:

(a) full chemical name—4,7,10,13,16,19-docosahexaenoic acid (22:6n-3 DHA);
(b) DHA (%)—minimum 32;
(c) trans fatty acids (%)—maximum 2.0;
(d) lead (mg/kg)—maximum 0.1;
(e) arsenic (mg/kg)—maximum 0.1;
(f) mercury (mg/kg)—maximum 0.1;
(g) hexane (mg/kg)—maximum 0.3.

S3–22 Specification for oil derived from marine micro-algae (Ulkenia sp.) rich in docosahexaenoic acid (DHA)

For oil derived from marine micro-algae (Ulkenia sp.) rich in docosahexaenoic acid (DHA), the specifications are the following:

(a) full chemical name for DHA—4,7,10,13,16,19-docosahexaenoic acid (22:6n-3 DHA);
(b) DHA (%)—minimum 32;
(c) trans fatty acids (%)—maximum 2.0;
(d) lead (mg/kg)—maximum 0.2;
(e) arsenic (mg/kg)—maximum 0.2;
(f) mercury (mg/kg)—maximum 0.2;
(g) hexane (mg/kg)—maximum 10.

S3–23 Specification for oxidised polyethylene

(1) In this section:

ASTM refers to standard test methods prepared by the American Society for Testing and Materials.

CAS means the Chemical Abstracts Service (CAS) Registry Number.

oxidised polyethylene (CAS 68441-17-8) is the polymer produced by the mild air oxidation of polyethylene.

(2) For oxidised polyethylene, the specifications are the following:

(a) average molecular weight—min 1200 (osmometric);
(b) viscosity at 125°C—min 200cP;
(c) oxygen content—max 9.1%;
(d) acid value—max 70 mgKOH/g (ASTM D 1386);
(e) drop point—min 95°C (ASTM D 566);
(f) density (20°C)—0.93-1.05 g/cm³ (ASTM D 1298, D 1505);
(g) extractable constituents:

(i) in water—maximum 1.5%; and
(ii) in 10% ethanol—max 2.3%; and
(iii) in 3% acetic acid—max 1.8%; and
(iv) in n-pentane—max 26.0%.

Note Extraction of oxidised polyethylene—25.0 g of finely ground oxidised polyethylene powder (particle size 300–1 000 μm) is extracted for 5 hours in the Soxhlet apparatus with 350 mL of solvent. The solvent is then distilled off and the distillation residue is dried in a vacuum oven at 80–90°C. After weighing the obtained residue, the components soluble in the solvent are calculated in % weight (based on the initial weight used).

S3–24 Specification for phytosterols, phytostanols and their esters

(1) Subject to subsections (2) and (3), phytosterols, phytostanols and their esters must comply with a monograph



Next Page →



Online Sources for this page:

Gazette.govt.nz PDF NZ Gazette 2015, No 50





✨ LLM interpretation of page content

🏥 Specification for oil derived from marine micro-algae (Schizochytrium sp.) rich in docosahexaenoic acid (DHA) (continued from previous page)

🏥 Health & Social Welfare
DHA, Marine micro-algae, Chemical specifications, Contaminants

🏥 Specification for oil derived from marine micro-algae (Ulkenia sp.) rich in docosahexaenoic acid (DHA)

🏥 Health & Social Welfare
DHA, Marine micro-algae, Chemical specifications, Contaminants

🏥 Specification for oxidised polyethylene

🏥 Health & Social Welfare
Oxidised polyethylene, Chemical specifications, Polymer, ASTM standards

🏥 Specification for phytosterols, phytostanols and their esters

🏥 Health & Social Welfare
Phytosterols, Phytostanols, Esters, Chemical specifications